- High conductivity of the copper coating improves efficiency and reduces heat generation.
- Typical composition is 95% graphite and 5% copper coating.
- Electric arcs efficiently melt the metal, with functional compressed air used to blow molten debris out of grooves.
- Our high-quality raw materials minimize dust and gases.
- The 1/8" diameter allows for shallow grooves and narrow width, offering more control in precise manual operations.
- The essential copper coating prevents breakage, overheating and oxidation in our standard gouging carbon electrodes.
- High conductivity of the copper coating improves efficiency and reduces heat generation.
- Typical composition is 95% graphite and 5% copper coating.
- Electric arcs efficiently melt the metal, with functional compressed air used to blow molten debris out of grooves.
- Our high-quality raw materials minimize dust and gases.
- The 1/8" diameter allows for shallow grooves and narrow width, offering more control in precise manual operations.